WARNING: This product can expose you to chemicals including Titanium dioxide (airborne, unbound particles of respirable size), which is known to the State of California to cause cancer, and Nitrous oxide, which is known to the State of California to cause birth defects or other reproductive harm. For more information go to www.P65Warnings.ca.gov.

0.035" ER5183 Hobart® MaxalMig® 5183 Aluminum MIG Wire 1 lb 4" Plastic Spool

Airgas Part #:HOB518303504

Hobart Brothers

Manufacturer #:518303504

SDS

Datasheet

Log in to get your price
$11.00 /US Pound
Package Size: 18 US pound
$11.00 US Pound
$11.00 US Pound
$198.00 Spool 18 US pound / Spool
$16,038.00 Pallet 1,458 US pound / Pallet

Typically in Stock

Item Details

  • 5183 filler metal is the most common aluminum/magnesium alloy for welding 5083 base metal in ship building applications. 5183 has higher strength values than 5356 with excellent salt water corrosion resistance when welded to 5083. Features/Benefits: - Very high strength (41 ksi typical) - High ductility/toughness/fatigue strength - Moderate ductility/formability - Lower electrical conductivity and thermal conductivity - Excellent corrosion resistance when welding 5083 base material - Higher column strength/better feedability - Very good color match after anodizing with 5xxx/6xxx base materials

Applications

  • 5083 and lower strength alloys (40 ksi minimum UTS), pressure vessels, shipbuilding, cryogenic tanks

Product Attributes

Diameter

» 0.035"

Weight

» 1 lb

AWS Classification

» ER5183

Trade Name

» Hobart® MaxalMig® 5183

Spool Diameter

» 4"

Package

» Plastic Spool